期刊文献+

T91钢Φ110mm管坯穿孔工艺生产实践 预览 被引量:1

Practice of T91 Steel Φ110 mm Billet Piercing Process
在线阅读 下载PDF
收藏 分享 导出
摘要 针对T91钢Φ110mm管坯热轧穿孔过程中顶头消耗高、连接接头脱丝或断裂及产品出现内折缺陷的问题,提出改进措施。分析认为:通过制定合理的加热制度,改进钼基顶头及连接接头结构,规范钼基顶头操作使用,可实现稳定生产,每个顶头平均穿孔支数达到363支,小时平均穿孔支数达67支左右,成本大幅下降。 Addressing the problems related to the piercing process of T91 steel Φ110 mm billets such as high consumption of plugs, loosing or breaking of plug connections, as well as the inner folds on pierced products, some countermeasures are proposed. It is indicated that by establishing a reasonable heating schedule, improving the structure of the molybdenum based plugs and connections, and standardizing the operation of the plugs, a stable piercing process with significantly lowerd cost can be realized when each plug may averagely pierce 363 billets in total and 67 billets per hour.
作者 金瞧童 JIN Qiaotong ( Jiangxi Hongdu Steel Works Co., Ltd., Nanehang 330013, China )
出处 《钢管》 CAS 2018年第3期43-45,共3页 Steel Pipe
关键词 T91钢 管坯 穿孔 工艺设计 加热制度 工具设计 T91 steel pipe billet piercing process design heating schedule tool design
作者简介 金瞧童(1985-),男,工程师,主要从事热轧钢管生产工艺技术、新产品开发及质量管理工作。
  • 相关文献

参考文献12

二级参考文献65

共引文献52

同被引文献12

引证文献1

投稿分析

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部 意见反馈